The Coloring and Texture of Concrete Products

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Coloring and Texture of Concrete Products

Author(s): Adolph Schilling

Publication: Journal Proceedings

Volume: 9

Issue: 12

Appears on pages(s): 491-497

Keywords: none

DOI: 10.14359/16149

Date: 12/1/1913

Abstract:
When, ten years ago, the speaker started to make concrete attractive and pleasing, he accepted as definitely settled its claim for strength and endurance, so thoroughly demonstrated by the enigneers of the time and the examples of ancient concrete work still in existence.