The Manufacture of Concrete Products is Germany

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Manufacture of Concrete Products is Germany

Author(s): Julius Carstanjen, Jr.

Publication: Journal Proceedings

Volume: 9

Issue: 12

Appears on pages(s): 480-487

Keywords: none

DOI: 10.14359/16148

Date: 12/1/1913

Abstract:
The artifical stone industry in Germany, which depended on the development of the cement industry, can be traced back for about 50 years. The cement at that time was quick setting, which made it possible to use the forms repeatedly, at short intervals. The method of manufacture consisted in casting the concrete, of very wet consistency, in wood and plaster forms.