The Constitution of Portland Cement. Some Results Obtained at the Experimental Cement Plant of the Bureau of Standards

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Constitution of Portland Cement. Some Results Obtained at the Experimental Cement Plant of the Bureau of Standards

Author(s): P.H. Bates

Publication: Journal Proceedings

Volume: 9

Issue: 12

Appears on pages(s): 368-377

Keywords: none

DOI: 10.14359/16135

Date: 12/1/1913

Abstract:
The constitution of Portland cement is at least a matter of considerable interest, if not of fundamental importance for the proper use. Notwithstanding the fact that this problem has been worked upon for a great number of years, yet it must be acknowledged that agreement among investigators is lacking to a great degree.