Tests of Waterproofing for Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tests of Waterproofing for Concrete

Author(s): Cloyd M. Chapman

Publication: Journal Proceedings

Volume: 9

Issue: 12

Appears on pages(s): 250-257

Keywords: none

DOI: 10.14359/16124

Date: 12/1/1913

Abstract:
So much that is contradictory has been said and wrriten concerning various methods of producing concrete which is waterproof and so much has been claimed by the vendors of various compounds which have been claimed by the vendors of various compounds which have been offered to the public as a postive solution of all waterproofing problems, that it is not surprising that not one cement user in ten has any definite or fixed opinion as to how to meet the problem of producing a waterproof concrete. There seems to be as many opinions on the subject as there are men willing to express their opinions.