Measurement of Actual Stresses in A Cantilever Flat Slab Reinforced Concrete Floor Having Rectangular Panels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Measurement of Actual Stresses in A Cantilever Flat Slab Reinforced Concrete Floor Having Rectangular Panels

Author(s): Arthur R. Lord

Publication: Journal Proceedings

Volume: 9

Issue: 12

Appears on pages(s): 127-150

Keywords: none

DOI: 10.14359/16119

Date: 12/1/1913

Abstract:
The Chicago Warehouse of the Larkin Company, in which the test described in this paper was made, is an eight-story and basment building of reinforced concrete construction throughtout. The building is 200 by 125 ft. in plan, divided into panels 20 ft. by 24 ft. 2 in. in dimension. The type of reinforced concrete construction used is that known as "Cantilever Flat Slab," and the designers the Concrete Steel Products Company of Chicago.