Title: Data on Lime Putty and Cream of Lime - Part II

Author(s): Cloyd M. Chapman

Publication: Journal Proceedings

Volume: 10

Issue: 12

Appears on pages(s): 465-469

Keywords: none

DOI: 10.14359/16111

Date: 12/1/1914

Abstract:
The points all fall very close to a curve which has been drawn in with a full line. It is apparent therefore from the close agreement between the points determined experimentally and the mathematically plotted curve that it is quite unnecessary to perform any experimental work in the laboratory to determine the amount of lime in a given volume of a lime putty of any consistency, provided the amount of water that has been mixed with a given weight of lime is known.