Title: Some Comparative Corrosion Tests of Plastered Metal Lath- A Progress Report

Author(s): J.C. Pearson

Publication: Journal Proceedings

Volume: 10

Issue: 11

Appears on pages(s): 445-458

Keywords: none

DOI: 10.14359/16107

Date: 11/1/1914

Abstract:
About three years ago the Bureau of Standards was requested by the Associated Metal Lath Manufacturers to co-operate with them in determining what factors play the most important part in bringing about the corosion and consequent failure of metal lath under stucco plaster.