Test of A Flat Slab Reinforced Concrete Floor at Shredded Wheat Factory, Niagra Falls, N.Y.

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Test of A Flat Slab Reinforced Concrete Floor at Shredded Wheat Factory, Niagra Falls, N.Y.

Author(s): W.A. Slater

Publication: Journal Proceedings

Volume: 10

Issue: 11

Appears on pages(s): 385-421

Keywords: none

DOI: 10.14359/16105

Date: 11/1/1914

Abstract:
The building tested, Fig.1, is a new factory building for the Shredded Wheat Company at Niagara Falls, N.Y. It was built by Braas Bros., contractors, Niagra Falls, N.Y.. According to plans reported by the Corrugated Bar Company of Buffalo, N.Y., and conforming to their standard practice. Mr. Walter McColloh acted as consulting engineer for the Shreded Wheat Company and supervised the construction of the building.