Title: Response of Plain Concrete to Cyclic Tension

Author(s): David Z. Yankelevsky and Hans W. Reinhardt

Publication: Materials Journal

Volume: 84

Issue: 5

Appears on pages(s): 365-373

Keywords: concretes; cracking (fracturing); crack width and spacing; cyclic loads; plain concrete; stress-strain relationships; tension; Materials Research

DOI: 10.14359/1610

Date: 9/1/1987

Abstract:
Cracking is an important feature of a concrete str