Recommended Practice for Concrete Architectural Stone, Building Block and Brick

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommended Practice for Concrete Architectural Stone, Building Block and Brick

Author(s): ACI Committee on Stone, Block and Brick

Publication: Journal Proceedings

Volume: 10

Issue: 8

Appears on pages(s): 352-357

Keywords: none

DOI: 10.14359/16097

Date: 8/1/1914

Abstract:
This recommended practice is intended to cover general requirements for the manufacture and testing of concrete architectural stone, building block and brick.