Combination of Reinforcement and Forms in Concrete Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Combination of Reinforcement and Forms in Concrete Construction

Author(s): T.W. Murray

Publication: Journal Proceedings

Volume: 10

Issue: 4

Appears on pages(s): 228-232

Keywords: none

DOI: 10.14359/16087

Date: 4/1/1914

Abstract:
Althought concrete construction dates back to the earliest days of history, it has been in the last decade only that a real development has been made in reinforced concrete construction, particularly in building work. The heavy masses of concrete and unscientific design of the reinforcement used in the earlier methods of concrete construction seem crude today.