The Expansion and Contraction of Concrete Roads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Expansion and Contraction of Concrete Roads

Author(s): R.J. Wig and W.S. Gefvert

Publication: Journal Proceedings

Volume: 10

Issue: 3

Appears on pages(s): 155-161

Keywords: none

DOI: 10.14359/16082

Date: 3/1/1914

Abstract:
The Bureau of Standards in connection with a general investigation of the volumetric changes which take place in concrete structures due to change in atmospheric temperature and moisture conditions made a number of measurements on concrete roads near New Village, N.J., and Nazareth, Pa., with the assistance of American Portland Cement Manufacturers.