Report of the Committee on Edison Fire

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of the Committee on Edison Fire

Author(s): ACI Committee on Edison Fire

Publication: Journal Proceedings

Volume: 11

Issue: 8

Appears on pages(s): 585-647

Keywords: none

DOI: 10.14359/16071

Date: 8/1/1915

Abstract:
Your Committee appointed to report the Edison fire, after a careful investigation of the characterof the buildings and their contents, the origin and intensity of the fire, have reached the following conclusions presented in the paper.