Reinforcing Narrow Concrete Roads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reinforcing Narrow Concrete Roads

Author(s): John W. Mueller

Publication: Journal Proceedings

Volume: 11

Issue: 4

Appears on pages(s): 91-96

Keywords: none

DOI: 10.14359/16045

Date: 4/1/1915

Abstract:
The subject of reinforcing concrete street pavements has already been thoroughly discussed, as evidence of which, reference may be made to the meeting of National Conference on Concrete Road Building in February, 1914. At that meeting practically every committee report referred to the necessity of reinforcing concrete pavements and roads, some advocating the practice to a greater extent than others on account of the particular subjects treated. . .