Title: The Construction of Integral Curbs

Author(s): Charles E. Russell

Publication: Journal Proceedings

Volume: 11

Issue: 3

Appears on pages(s): 78-83

Keywords: none

DOI: 10.14359/16043

Date: 3/1/1915

Abstract:
All street pavements call for some form of curb and gutter, the cost of which to property owners usually amounts to from 45 to 90 cents per linear foot of street frontage, an expenditure often equivalent to 25 per cent of the cost of the pavement proper.