Some Further Results Obtained in Investigating Properties of Portland Cements Having a High MgO Content

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Some Further Results Obtained in Investigating Properties of Portland Cements Having a High MgO Content

Author(s): P.H. Bates

Publication: Journal Proceedings

Volume: 11

Issue: 1

Appears on pages(s): 89-107

Keywords: none

DOI: 10.14359/16033

Date: 1/1/1915

Abstract:
This paper contains further data concerning high Magnesium Portland cements, obtained from cements burned in the experimental plant of this Bureau. It contains the results obtained from a second series of burns, as well as later tests of the physical specimen of the first series reported at the last meeting of this Institute. The same prodcedure was followed in the present series as in the first, but in the present investigation the composition was changed so that the resulting cements have a lower limemagnesia content and a higher silica and higher alumina-iron oxide content.