Proposed Revised Recommended Practice for Plain Concrete Pipe and Drain Tile

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revised Recommended Practice for Plain Concrete Pipe and Drain Tile

Author(s): ACI Committee on Recommended Practice for Plain Concrete Pipe and Drain Tile

Publication: Journal Proceedings

Volume: 11

Issue: 1

Appears on pages(s): 70-76

Keywords: none

DOI: 10.14359/16030

Date: 1/1/1915

Abstract:
This recommended practice is intended to cover general requirments for the manufacture of plain concrete pipe and drain tile.