Title: Proposed Specifications for Manufacture of Concrete Sewer Pipe by Machine

Author(s): ACI Committee on Specifications for Manufacture of Concrete Sewer Pipe by Machine

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 496-498

Keywords: none

DOI: 10.14359/16020

Date: 2/1/1916

Abstract:
1. Portland Cement.- The cement shall meet the requirements of the Standard Specifications for Portland Cement of the American Society for Testing Materials, adopted August 16, 1909, as revised to date by said Society.