Title: Report of Committee on Specifications and Methods of Tests for Concrete Materials for 1916

Author(s): ACI Committee on Specifications and Methods of Tests for Concrete Materials for 1916

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 478-479

Keywords: none

DOI: 10.14359/16016

Date: 2/1/1916

Abstract:
In the report of last year described the co-ordination of the work of your committeewith that of C-9 of the American Society for Testing Materials. As a result of the joint action thus made possible, the work has been extended and broadened, and funds have been provided for research.