Title: Concrete Foundations for Asphalt Pavements and Roads Subject to Heavy Travel

Author(s): Clifford Richardson

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 465-467

Keywords: none

DOI: 10.14359/16012

Date: 2/1/1916

Abstract:
The first essential in road construction of a permanent character is a dry and firm subsoil upon which to build.