Title: Report of Committee on Fireproofing

Author(s): ACI Committee on Committee on Fireproofing

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 335-338

Keywords: none

DOI: 10.14359/15996

Date: 2/1/1916

Abstract:
The most important item of the work before this committee is the question of fire protection for columns in fire-resisting buildings. This necessarily follows from the structural importance of the column, nd the disastrous results if it fails.