Title: The Flow of Concrete Under Sustained Load

Author(s): Earl B. Smith

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 317-321

Keywords: none

DOI: 10.14359/15994

Date: 2/1/1916

Abstract:
The ordinary conception of the behavior of materials of construction under stress is that it follows Hooke's law for both increasing and decreasing loads within the limit of elasticity.