Time Tests of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time Tests of Concrete

Author(s): Almon H. Fuller and Charles C. More

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 302-310

Keywords: none

DOI: 10.14359/15993

Date: 2/1/1916

Abstract:
In making a recent test (April, 1915) of a reinforced concrete building the writers found concrete deformation in the building which greatly exceeded those in the laboratory tests, under, presumably, approximately the same unit stresses. It was found, further, that the deformation in the building increased during the few days that the maximum test load was allowed to remain. It seemed probable, therefore, that the time element should be considered in interpreting the stresses, but a search in available literature failed to disclose any data on the subject.