Title: Tets on Concrete Columns, Plain and Reinforced

Author(s): Frank P. McKibben and A.S. Merrill

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 200-240

Keywords: none

DOI: 10.14359/15990

Date: 2/1/1916

Abstract:
This paper records the results of tests on 33 concrete columns made in the Friz Engineering Laboratory by the civil engineering department of Lehigh University.