Reinforced Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reinforced Concrete Columns

Author(s): Pierce P. Furber

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 181-199

Keywords: none

DOI: 10.14359/15989

Date: 2/1/1916

Abstract:
The report of column tests by the Committee of the American Concrete Institute (see Journal, American Concrete Institute, Februray, 1915, p. 47) is instructive, as it enbables one to show by comparision that most of the building ordinances now in effect are far from correct in their specifications for unit stresses on hooped columns. Being published nearly simultaneous with accounts of the Edison fire, this report brought the subject of concrete columns vividly to the attention of those in the buidling business, regarding questions of both safde loads and fire resistance.