Construction of Kensico Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction of Kensico Dam

Author(s): Wilson Fitch Smith

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 147-170

Keywords: none

DOI: 10.14359/15987

Date: 2/1/1916

Abstract:
The Kensico Dam of the Catskill Water Supply System of the City of New York is an engineering work of considerable interest, not only on account of its size and the remarkable progress that was made in its construction, but because it is the first large dam in this country to receive serious architectural treatment.