A Study on the Calcium Chloride Resistance of Concrete Containing an Expansive Additive

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Study on the Calcium Chloride Resistance of Concrete Containing an Expansive Additive

Author(s): H. Akihiro, A. Masanobu, K. Hiroyuki, and F. Tsutomu

Publication: Symposium Paper

Volume: 234

Issue:

Appears on pages(s): 431-444

Keywords: calcium chloride resistance; low dosage of expansive additive; ordinary expansive additive

DOI: 10.14359/15950

Date: 3/22/2006

Abstract:
In this paper, the calcium chloride resistance of concrete containing a low dosage of an expansive additive was investigated in comparison to that of plain concrete. To evaluate the chloride resistance, the length of change and compressive strength, EPMA and SEM were used. In addition, comparisons with previous results on chloride resistance of concrete with ordinary expansive additive were also confirmed.