Standard Specifications for One-Course Concrete Alley Pavement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Standard Specifications for One-Course Concrete Alley Pavement

Author(s): ACI Committee on Specifications for One-Course Concrete Alley Pavement

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 449-456

Keywords: none

DOI: 10.14359/15908

Date: 2/1/1917

Abstract:
Adopted by Letter Ballot on April 10, 1917. Specifications include: materials, grading, drainage, subgrade, forms, pavement section, joints, measuring materials and mixing concrete, reinforcing, placing concrete, and protection.