Standard Specificatins for One-Course Concrete Street Pavement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Standard Specificatins for One-Course Concrete Street Pavement

Author(s): ACI Committee Standard No. 17

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 432-439

Keywords: none

DOI: 10.14359/15904

Date: 2/1/1917

Abstract:
Adopted by Letter Ballot on April 10, 1917. Specifications include: materials, grading, drainage, subgrade, forms, pavement section, joints, measuring materials and mixing concrete, reinforcing, placing concrete, protection, and shoulders.