Title: Proposed Standard Specifications for Monolithic Concrete Sewers and Recommended Rules for Concrete Sewer Design

Author(s): ACI Committee on Concrete Sewers

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 371-385

Keywords: none

DOI: 10.14359/15898

Date: 2/1/1917

Abstract:
The materials required for the construction shall be furnished by the contractor and will be inspected by the enigeer.