Proposed Revised Specifications for Concrete Floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revised Specifications for Concrete Floors

Author(s): ACI Committee on Sidewalks and Floors

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 358-365

Keywords: none

DOI: 10.14359/15896

Date: 2/1/1917

Abstract:
These specifications apply to floors in buildings, whether subjected to moderate or heavy traffic, and cover the laying and finishing of the floor; also its protection during early hardening.