Title: Proposed Revised Specifications for Conrete Sidewalks

Author(s): ACI Committee on Sidewalks and Floors

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 351-357

Keywords: none

DOI: 10.14359/15895

Date: 2/1/1917

Abstract:
These specifications apply to concrete sidewalks in residence and business districts, and cover the preparation of the sub-base, the laying and finishing of the walk and its protection during early hardening.