Abstract:
As artisans in concrete, let us give a few thoughts as to what are ornamental products. My idea is that such products are columns and capitals, urns, railings and balustrades, cornices and cornice ornaments, entablatures, window trim, decorative panels, cartouches, garden furniture, lamp standards, and in fact anything that is used to decorate or ornament a building, cemetery, park or private grounds.