The Influence of Total Width of the Effective Width of Reinforced-Concrete Slabs Subjected to Cental Concentrated Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Influence of Total Width of the Effective Width of Reinforced-Concrete Slabs Subjected to Cental Concentrated Loading

Author(s): A.T. Goldbeck

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 78-88

Keywords: none

DOI: 10.14359/15865

Date: 2/1/1917

Abstract:
About five years ago the United States Office of Public Roads increased the scope of its activities by adding a bridge department to its organization.