Title: Sidewalks and Floors

Author(s): ACI Committee on Concrete Sidewalks and Floors

Publication: Journal Proceedings

Volume: 14

Issue: 6

Appears on pages(s): 486-503

Keywords: none

DOI: 10.14359/15829

Date: 6/1/1918

Abstract:
Since the last report of the committee specifications for sidewalk construction have been secured from over a hundred cities throughout the country, digest of which has been prepared and made a part of this report.