Title: Reinforced Concrete and Building Laws

Author(s): ACI Committee on Reinforced Concrete and Building Laws

Publication: Journal Proceedings

Volume: 14

Issue: 6

Appears on pages(s): 481

Keywords: none

DOI: 10.14359/15827

Date: 6/1/1918

Abstract:
At the meeting of the American Concrete Institute in Chicago in February, 1917, a proposed Standard Building Regulation for the Use of Reinforced-Concrete was submitted for adoption. During the past year some very valuable data have been obtained from several tests.