Problems Arising in the Design and Construction of Reinforced Concrete Ships

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Problems Arising in the Design and Construction of Reinforced Concrete Ships

Author(s): R.J. Wig and S.C. Hollister

Publication: Journal Proceedings

Volume: 14

Issue: 6

Appears on pages(s): 441-464

Keywords: none

DOI: 10.14359/15824

Date: 6/1/1918

Abstract:
It is presumptuous to attempt to outline in any complete manner the problems which are to be met in the design and construction of concrete ships before we have had the actual experience of completing the construction of some such ships.