Title: Ornamental and Decorative Concrete

Author(s): R.F. Havlik

Publication: Journal Proceedings

Volume: 14

Issue: 6

Appears on pages(s): 240-249

Keywords: none

DOI: 10.14359/15797

Date: 6/1/1918

Abstract:
Decorative concrete may be divided into the following three classes: (1) Concrete garden furniture; (2) Concrete trim stone and decorations for buildings; (3) Decorative mass concrete. The third class is largely one of design and is applicable to any concrete work.