Title: A Test of the S-M-I System of Flat-Slab Construction

Author(s): Edward Smulski

Publication: Journal Proceedings

Volume: 14

Issue: 6

Appears on pages(s): 206-232

Keywords: none

DOI: 10.14359/15795

Date: 6/1/1918

Abstract:
The subject of this paper is the test of a slab, designed according to the S-M-I or Smulski System, made by Prof. W.K. Hatt at Purdue University, and the theorectical discussion of the action of rings in resisting bending moments. The main data of the test are taken directly from Professor Hatt's report, for which due credit to him is hereby given.