Amendments to Recommended Practice for Concrete Roads and Street Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Amendments to Recommended Practice for Concrete Roads and Street Construction

Author(s): ACI Committee on Concrete Roads and Pavements

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 405-410

Keywords: none

DOI: 10.14359/15784

Date: 6/1/1919

Abstract:
The cuts shown in the report are revisions of drawings of the same figure in the Proceedings. . .