Title: Report of the Committee on Reinforced-Concrete Highway Bridges and Culverts

Author(s): ACI Committee on Reinforced-Concrete Highway Bridges and Culverts

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 360-372

Keywords: none

DOI: 10.14359/15779

Date: 6/1/1919

Abstract:
The work of the Committee on Highway Bridges and Culverts during the past four months is given herewith as a matter of record since a late start and the impossibility of a meeting of its membership to discuss the data collected precluded definite recommendations of the full program contemplated.