Report of Committee on Treatment of Concrete Surfaces

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of Committee on Treatment of Concrete Surfaces

Author(s): Comittiee

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 343

Keywords: none

DOI: 10.14359/15777

Date: 6/1/1919

Abstract:
Your committee has for some time been considering the advisiability of preparing a Standard Recommended Practice for Portland Cement Stucco.