Title: Method of Construction of Concrete Ships

Author(s): R.J. Wig

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 241-288

Keywords: none

DOI: 10.14359/15771

Date: 6/1/1919

Abstract:
This paper is confined to a description of the methods employed in the construction of concrete ships for the United States Shipping Board Emergency Fleet Corporation. The complete program of the Fleet Corporation comprises the construction of 14 ships of five different types.