Title: Layout and Equipment of the Government Concrete Shipyards

Author(s): A.L. Bush

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 216-230

Keywords: none

DOI: 10.14359/15769

Date: 6/1/1919

Abstract:
The United States Shipping Board, Emergency Fleet Corporation, adopted its program for constructing concrete ships at a time when speed in construction was considered one of the most important factors.