Title: Effect of Vibration, Jigging and Pressure on Fresh Concrete

Author(s): Duff A. Abrams

Publication: Journal Proceedings

Volume: 15

Issue: 6

Appears on pages(s): 63-85

Keywords: none

DOI: 10.14359/15759

Date: 6/1/1919

Abstract:
An experimental study of the effect of vibration and pressure on fresh concrete on its strength and other properties is of interest in view of the frequent use of such devices as hand-hammering of forms, or air-hammering, jigging or vibration as an aid in placing concrete.