Standardizing the Specifications for Steel Bars for Concrete Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Standardizing the Specifications for Steel Bars for Concrete Reinforcement

Author(s): ACI Committee on Standardizing the Specifications for Steel Bars for Concrete Reinforcement

Publication: Journal Proceedings

Volume: 16

Issue: 2

Appears on pages(s): 239-240

Keywords: none

DOI: 10.14359/15753

Date: 2/1/1920

Abstract:
The committee presented a report which, after discussion, was modified on the floor to read as follows: A reduction in the number of areas with equivalent sizes of concrete reinforcing bars was recommended by the War Service Committee on Reinforcement to the United States War Industries Board during the summer and fall of 1918, as a conservation measure, which would have been adopted by the Government, had the war continued.