Title: Aggregates

Author(s): ACI Committee on Concrete Aggregates

Publication: Journal Proceedings

Volume: 16

Issue: 2

Appears on pages(s): 230-233

Keywords: none

DOI: 10.14359/15752

Date: 2/1/1920

Abstract:
This committee, working in close co-operation with Committee C-9 on Concrete and Concrete Aggregates of the American Society for Testing Materials, has had the progress of its work seriously interfered with by the active participation of many of its members in Government work, and more recently by urgently pressing business demands and lack of assistants in laboratories.