Compressive Strength of Concrete in Flexure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compressive Strength of Concrete in Flexure

Author(s): W.A. Slater and R.R. Zipprodt

Publication: Journal Proceedings

Volume: 16

Issue: 2

Appears on pages(s): 120-146

Keywords: none

DOI: 10.14359/15741

Date: 2/1/1920

Abstract:
For calculations of strength in the design of reinforced-concrete beams, the use of the "straight line" formula has become almost universal. In adopting this formula it has been generally recognized that the compressive stresses calculated by its use were greater than those actually developed under the conditions assumed.