Wear and Compression Tests of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Wear and Compression Tests of Concrete

Author(s): Ray B. Crepps

Publication: Journal Proceedings

Volume: 16

Issue: 2

Appears on pages(s): 108-117

Keywords: none

DOI: 10.14359/15740

Date: 2/1/1920

Abstract:
This paper gives results and curves taken from a series of tests conducted in the Testing Materials Laboratory of Purdue University in cooperation with the Indiana Sand and Gravel Producers Association. The tests were originally designed with a view of placing before the members of that association some underlying principles in concrete mixtures. However, a number of tests taken from the different series are comparable under this heading.