Report of Committee on Concrete Bridges and Culverts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Report of Committee on Concrete Bridges and Culverts

Author(s): ACI Committee on Concrete Bridges and Culverts

Publication: Journal Proceedings

Volume: 17

Issue: 2

Appears on pages(s): 301

Keywords: none

DOI: 10.14359/15721

Date: 2/1/1921

Abstract:
The Committee on Concrete Bridges and Culverts is unable to report any definite recommendations on the program which is being considered as outlined in the 1920 "Proceedings" of the Institute. Much data has been collected, and this will be complied and recommendations made. It reports some constructive work in an endeavor to establish a permanently active organization by which it will be possible to carry on the important work under construction in authoritative manner.